Cuprothal 10, CuNi6, NC6.
Votoaty simika,%
Ni | Mn | Fe | Si | Cu | hafa | ROHS Directive Cd | ROHS Directive Pb | Torolàlana ROHS Hg | ROHS Directive Cr |
---|---|---|---|---|---|---|---|---|---|
6 | - | - | - | Bal | - | ND | ND | ND | ND |
Toetra mekanika
Anaran'ny fananana | sarobidy |
---|---|
Max Continuous Service Temp | 200 ℃ |
Resisivity amin'ny 20 ℃ | 0.1±10%ohm mm2/m |
hakitroky | 8,9 g/cm3 |
Conductivity mafana | <60 |
Tarehin-tsetroka | 1095 ℃ |
Herin'ny tensile, N/mm2 Anelina, Malefaka | 170~340 Mpa |
Henjana, N/mm2 Cold Rolled | 340~680 Mpa |
Elongation (anneal) | 25% (Min) |
Elongation (cold rolled) | 2% (Min) |
EMF vs Cu, μV/ºC (0~100ºC) | -12 |
Magnetika fananana | tsy |